Home/Reference

Which mark stays on which surface

Reference · compatibility8 min readPublished 27 Nov 2026Sources: published surface-energy data · dyne-testing practice
The short answer

Whether a mark survives is decided by three properties: surface energy (does the ink wet it), porosity (does anything absorb it), and heat tolerance (can a laser mark it). None of the three can be read off a datasheet reliably — they vary by grade, additive and age. Measure the actual material with a dyne pen, a drop of water and, if laser is on the table, a test mark.

The three tests that decide

Each property has a cheap, fast test you can run on the production floor — before any vendor visit:

Surface energy
Dyne pen, or a marked range of pens. Ink only wets a surface whose energy meets or beats the ink's surface tension — a bead of ink on the surface is the failure in miniature.
Porosity
A drop of water. Soaks in within seconds: porous, absorbent inks are fine. Sits on top and beads: non-porous, the ink must set by evaporation or cure instead.
Heat tolerance
A laser test mark on production material. The question is not only contrast, but what the heat did — discoloration, embrittlement, or a mark through to the other side.

The dyne number deserves one caution: it is a measurement of a condition, not a property. Extruded film leaves the line treated, spends three weeks in a warm warehouse, and arrives with a lower dyne level than its datasheet claims. Measure the roll at your line, not the brochure's figure.

The compatibility table

Starting points, not verdicts. Every cell assumes the ink family matched to the substrate — the pairing logic is in the section below.

SubstrateSolvent CIJTIJTTOLaserField note
PE / XLPE (untreated)Only inks made for low-energy surfacesPoor—Often the best optionRoughly 31 mN/m; the reason cable lines pretreat or go laser. See the XLPE guide.
PP filmMatched inksPoor untreatedYes (contact)With careSimilar energy to PE — roughly 29–31 mN/m untreated; corona-treated films print well.
PET filmUsually goodOften goodYesAdditive for contrastCommonly reported in the low-to-mid 40s mN/m untreated — measure, treatments vary.
PVC (rigid)GoodGoodYesPossible, watch gasesAround 39 mN/m — takes most solvent inks without pretreatment.
GlassFast-set inksFair—Yes (CO₂)High energy but non-porous; adhesion is about cure speed, not wetting.
Metal, bareGood with matched inkFair—Yes (fiber)High energy — but mill oils defeat everything. Clean first; oil is the usual culprit.
Metal, painted / coatedDepends on coatingDepends—OftenThe paint is the substrate. Test the coating, not the metal.
Paper & board (uncoated)GoodPenetrating inksYesCharring contrastAbsorption locks the mark in; kraft needs contrast, not adhesion.
Coated boardFast-set inksNon-penetrating inksYesYesThe coating decides: penetrating inks smear on top of it — the pharma DataMatrix case. See the pharma guide.
Rubber / elastomerSpecialty inksPoor—Depends on fillerLow energy, flexes and sheds marks; slip additives migrate and defeat adhesion over weeks.
LSZH compoundsSpecialty inksPoor—VariesFiller-rich compounds steal ink and scatter laser. See the LSZH page.

Categories are starting points. Grade, additives and age move every row by a margin that only a dyne pen and a rub test on production material can measure. Where a cell says "with care" or "depends", that is the honest answer — treat any vendor claim of "prints on anything" as a promise to test.

What pretreatment changes

Corona, flame and plasma all do the same job — raise the surface energy of the outermost molecular layer so ink can wet it. Three things worth knowing before you specify one:

  1. The effect is temporary. Treated surfaces decay in storage — weeks to months depending on material, additive package and conditions. A film treated at the film plant and printed two months later may measure below its ink's wetting threshold. Treatment and printing belong close together in time.
  2. It adds a machine and a failure mode. The treater has electrodes, width limits and speed ranges; misalignment shows up as print failure two stations downstream. When adhesion drifts on a treated line, check the treater before blaming the ink.
  3. It competes with laser on economics. On substrates like XLPE, a laser needs no consumables and no treatment station — which is why low-energy products so often end up laser-marked. The comparison belongs in the five-year cost worksheet, not the datasheet.

Ink families and what they want

FamilyBonds byWantsHates
MEK / acetone solvent (CIJ)Solvent bite + resin bondingNon-porous plastics, fast line speedsPorous stocks that over-absorb; solvent-restricted rooms
Alcohol-basedMild biteFood and pharma areas where MEK is unwelcomeLow-energy surfaces; slow evaporation in humid air
Water-basedAbsorption into porous stockPaper, board, uncoated stocksPlastics — it beads and never sets
Penetrating TIJSoaking in, then dying into the fibreUncoated paper and boardCoated surfaces — it stays on top and smears
Non-penetrating / fast-set TIJQuick surface setCoated board, films, plasticsVery absorbent stocks; slow set in cold rooms
UV-curable (TIJ/PIJ)Photochemical cureNon-porous surfaces needing instant handlingShadows (the cure needs light); substrate flexibility limits

The families, not the brands, decide what is possible. Within a family, adhesion promoters and pigments vary — which is why the final arbiter is always a test on your material.

The rub test that settles it

Every compatibility argument ends the same way: print on production material, at production settings, then apply the two tests the rest of this site uses:

  1. Dry rub — twenty firm strokes with a dry cotton cloth. Simulates handling and packing.
  2. IPA wipe — ten wipes with 70% isopropyl alcohol. Simulates the cleaning, the downstream process, or the customer's thumb and a sanitiser.

A mark that survives both on the worst material lot you can find is compatible. Everything before that test is marketing.

Write it into the order

"The mark shall remain legible after 20 strokes of a dry cotton cloth at firm pressure and 10 wipes with 70% IPA, at minimum and maximum line speed, on production material." This is the same adhesion clause used in acceptance testing — with a method attached, it can be enforced.

Questions we get

The datasheet says our film is corona-treated. Is that enough?

Treatment decays — sometimes to below the ink's wetting threshold by the time the roll reaches your line. Measure dyne on the roll as it sits at the coder, not the value on the film datasheet. If it reads low, either treat at the line or move the print point closer to the treatment date.

Why does the same ink work on one batch and fail on the next?

Formulation changes upstream: slip additives, antistatic agents, a new stabiliser package. None of them change how the film looks; all of them change what happens at the surface. Re-run the dyne pen on the failing lot — it usually explains the failure in five minutes.

Can one ink cover all our substrates?

Rarely, and the cost of forcing it shows up as marginal marks on the difficult substrates. Shortlist by family per substrate class, then test the specific pair. A line with both porous cartons and low-energy film will almost always need two ink systems.

What does laser need from a substrate?

Heat tolerance and a contrast response — charring, foaming, bleaching or colour change. If the material responds weakly, additives can help (and add a consumable back). Test on production material: the same polymer in a different colour or filler can behave completely differently under the beam.

Is dyne testing destructive?

The pens leave a small trace on the tested spot, so test on waste areas or offcuts, not on saleable product. The pens themselves also age — an open pen is no longer a reference. Replace them regularly or calibrate against known films.

Related

Also in reference

Pages that connect to this one.

This page
Why ink fails on XLPE

Surface energy, line speed and the cable case in full.

Cable
LSZH compounds

The filler problem taken to its extreme.

Cable
CIJ vs TIJ vs TTO vs laser

The method-by-method comparison behind the columns above.

Comparison
Acceptance testing a coding line

Where the adhesion clause belongs in the contract.

Contract